Effects of Solution Treatment on Microstructure and Mechanical Properties of Differential Pressure Casting GW103K Alloy

Qilong Wang,Guohua Wu,Zhengquan Hou,Bin Chen,Yun Zheng,Wenjiang Ding
DOI: https://doi.org/10.3870/tzzz.2009.03.013
2009-01-01
Abstract:Microstructure, mechanical properties, fracture morphology and fracture mechanism of differential pressure casting Mg-10Gd-3Y-Zr alloy with solution treatment were investigated by optical microscope (OM), scanning electron microscope (SEM), X-ray diffraction (XRD) and tensile testing. The results show that grain size in the microstructure is increased from 73 μm to 90 μm, and hardness as wel as yield strength is firstly increased then decreased and then increased with solution temperature increasing from 500°C to 535°C. Microstructure of T4 treated alloy is composed of α-Mg solid solution and cuboidal particles with rich (Gd + Y) phase, whose tensile strength, yield strength and elongation are 231MPa, 149MPa and 4. 8%, respectively, after solution treatment at 535°C for 10 hours, exhibiting desirable comprehensive mechanical properties. The fracture morphology of the T4 treated alloy is characterized by intergranular and transgranular fracture combining with limited cleavage fracture.
What problem does this paper attempt to address?