EFFECT OF PRE-OXIDATION ON CATALYTIC CRACKING PERFORMANCE OF COKER GAS OIL

Xiu-jie MEN,Bin SHI,Dao-yong YU,Guo-he QUE
DOI: https://doi.org/10.3969/j.issn.1001-8719.2008.03.006
2008-01-01
Abstract:Kelamay coker gas oil (KLCGO) pre-oxidized by potassium permanganate (KMnO 4) in an autoclave was analyzed by vapor pressure osmometry (VPO) for the change of its mean relative molecular mass and FT-IR for that of its function groups, along with study of its catalytic cracking performance on a simulated fixed-bed apparatus. The results showed that pre-oxidizing of KMnO 4 resulted in the new oxygenic groups and the decrease of mean relative molecular mass from 300 to about 250, and the catalytic cracking was improved by the increase of the total conversion and the light oil production about 3.33% and 7.73% while the decrease of dry gas and coke yield about 0.52% and 1.08%, respectively. The appropriate dosage of KMnO 4 for pre-oxidation to upgrade KLCGO was 1500 μg/g.