Weld movement of tailor-welded tube hydroforming

Guan-nan CHU,Xiao-song WANG,Gang LIU,Shi-jian YUAN,Jian-guo GE
DOI: https://doi.org/10.3969/j.issn.1005-0299.2008.01.007
2008-01-01
Abstract:To reveal the weld movement phenomenon in hydroforming of tailor-welded tubes with different thicknesses, FEM simulations were carried out to analyze the effects of internal pressure, thickness ratio, length ratio, friction coefficient and hardening coefficient on weld movement. The result indicates that weld movement appears during tailor-weld tube hydroforming. Consequently, obvious thinning happens near the weld seam on the thinner tube. Weld movement increases with the increasing of thickness ratio and length ratio, but decreaseds with the increasing of friction coefficient and hardening coefficient. To reduce the weld movement, the reasonable structure of the tailor-welded tubes should be designed with thickness ratio lower than 2.0 and length ratio lower than 3.5.