Abstract:SrNdCoO 4 ceramics with tetragonal K 2 NiF 4 structure were prepared by a solid-state reaction process. The frequency and temperature dependence of dielectric and conductive properties were studied. A peak was found at ∼325 °C on both dielectric constant ( ɛ ) and conductivity ( σ ) plots with temperature. After annealing in O 2 , the peak of ɛ disappeared while that of σ just shifted a little toward high temperature side. So, some oxide vacancies existed in the polycrystalline SrNdCoO 4 , which contributed much to ɛ but influenced σ only slightly in the measured temperature and frequency range. A lower resistivity of 3.7 Ωcm was obtained in SrNdCoO 4 ceramics sintered at 1150 °C.