Abstract:Homemade 3Y-TZP submicrocrystalline powder was selected to investigate the effect of burning out of binder for 24 h on the mechanical properties of pre-sintered ceramic specimens by bidirectional dry-press and iso-static-hydraulic press to overcome the sintering bent of bar-shaped specimens. The temperature vs. expansion curve of pre-sintered specimens was determined, and the densities of specimens at different sintering temperatures were compared, and XRD quantitative analysis was used to confirm the sintering schedule. The results show that the flexural strength and fracture toughness of pre-sintered specimens are not affected by the burning out of binder. The adequate flexural strength and fracture toughness can be got when the specimens were pre-sintered at a higher temperature of 1550 degrees C for 0.5 h for type-I dental ceramic.
What problem does this paper attempt to address?