Abstract:ZnGa2O4:Cr3+ red phosphors were synthesized by citric-gel method. Typical spinel-phase ZnGa2O4 could be attained after calcined at 1000 degrees C in air ambient. According to the results of XPS and EPR, it could be deduced that Cr3+ ions were dominant in the lattice and it could not be oxidized to Cr5+ or Cr6+ after calcined in air. The emission of Cr3+ at 695 nm is originated from the transition of E-2-(4)A(2). And due to the large overlap between absorption band of Cr3+ and emission band of the host, Cr3+ could obtain the excitation energy from the host via the effective energy transfer. The electroluminescent device was. fabricated by screen printing utilizing ZnGa2O4 :Cr3+ as the phosphor layer. Luminance (L) versus voltage (V) of the device match the well-known equation of L=L(o)exp(-bV(-1/2)) and the luminance increase proportionally with frequency due to the increase of excitation probability of host lattice or Cr3+ centers. The diagram of charge density (Q) versus applied voltage (V) is based on a conventional Sawyer-Tower circuit. At 280 V and 1000 Hz, the luminance and luminous efficiency of the fabricated powder EL device are about 1.0 cd . m(-2) and 13 lm . W-1, respectively.
What problem does this paper attempt to address?