Study on superplasticity of Ti-10V-2Fe-3Al powder alloy

Chunyan Duan,Hongzhen Guo,Huiping Tang,Zekun Yao,Haiyan Liu,Wei Zhang,Zhanglong Zhao
2005-01-01
Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering
Abstract:In this paper the Ti-10V-2Fe-3Al powder alloy has been prepared by powder sintering + isothermal forging. Its relative density can reach 99.57%. Homogeneous and fine-grained microstructures can be obtained and the equiaxed degree of primary α phases is satisfied. Therefore, the powder alloy presents excellent superplasticity. The average elongation is 1269%, and the maximum value is 1422% (that of normal cast + forged alloy is 676%). The process is an effective way to refine the microstructure and to improve the superplastic property. The result of superplastic tensile test indicates that Ti-10V-2Fe-3Al powder alloy presents the superplasticity in the range of temperature from 700°C to 820°C and of strain rate from 3.3×10-4s-1 to 3.3×10-2s -1. The optimal superplastic deformation conditions are 750°C-760°C and 3.3×10-4s-1-3. 3×10-3s-1, under which the elongation can reach 1269%-1422% and the flow stress is 23.6 MPa-62.3 MPa. Under optimal superplastic deformation conditions the tensile specimens present the fracture in the form of point and the fracture surface fluctuates greatly. It shows obvious intergranular fracture.
What problem does this paper attempt to address?