INFLUENCE OFFLLUX ADDITIVES ON THE LUMINESCENT PROPERTIES OF Y2 O2 S:TILONG AFTERGLOW PHOSPHOR

ZHANG Pengyue,HUANG Qiuping,CHENG Haobo,FAN Xianping,WANG Xhiyu,QIAN Guodong,WANG Minquan
DOI: https://doi.org/10.3321/j.issn:0454-5648.2005.02.002
2005-01-01
Abstract:A long afterglow phosphor of Y2O2S∶0.09Ti without rare earth activation ion was synthesized by high temperature solid state reduction method. The influence of five fluxes of Li2CO3, Na2CO3, K2CO3, K3PO4 and K2HPO4 on luminescent properties of Y2O2S∶Ti phosphor was investigated. The results indicate that single phase Y2O2S∶Ti could be obtained by adding Li2CO3,Na2CO3, K2CO3 or K3PO4 as flux except K2HPO4 . The emission spectra show that the intensity of emission peak at 565 nm depends greatly on the added flux. Furthermore, afterglow brightness of Y2O2S∶Ti is enhanced by adding the flux, especially adding the Li2CO3 increases the afterglow brightness to 10.1 mcd/m2 at decay time of 10 min compared with the K2CO3, 0.15 mcd/m2. The phosphor added with Li2CO3 yields the afterglow with yellow color lasting over 5 h with recognizable intensity level (0.32 mcd/m2) after the removal of the excitation light at darkroom.
What problem does this paper attempt to address?