Study on High-Temperature and Moist Resistant Properties of Glass Fiber/methylsilicone Composites

郭旭,黄玉东,曹海琳
DOI: https://doi.org/10.3969/j.issn.1005-5053.2004.04.011
2004-01-01
Abstract:The interlaminar shear strength (ILSS) under high temperature and moist resistance of glass fiber/methylsilicone (GF/ methylsilicone )composites were investigated. The results show that the ILSS gradually decreased with increase of ignition temperature between room temperature to 800℃, but it is constant during 800~1000℃. The structure of methylsilicone resin at different temperature was characterized by IR spectrum. It is shown that the structure of methylsilicone resin was stable until 800℃.The thermal stability of methylsilicone was studied by TG, the result shows that it has good heat resistant. Meanwhile the interface structure of the composites at 800℃ was investigated by means of SEM. The moist heat resistance testing shows that the water absorption being only (2.35%) and ILSS decreasing by 21.9% after boiling for 100h.