CdS THIN FILMS FABRICATED BY CHEMICAL BATH DEPOSITION

张辉,杨德仁,马向阳,阙端麟
DOI: https://doi.org/10.3321/j.issn:0254-0096.2003.01.001
2003-01-01
Abstract:Cubic phase CdS thin films have been prepared by chemical bath deposition (CBD). The CdS film precursors were deposited on ITO glass without stirring and sodium citrate using as the complexing agent by the solution consisting of 0.02 mol/L CdCl2, 0.02 mol/L sodium citrate and 0.05 mol/L CS(NH2)2 with pH 11.5 and temperature of 80°C. And the thin films were then annealed at 350°C for 2 h in N2 gas. X-ray diffraction (XRD) patterns and Scanning electron microscopy (SEM) images indicate that the deposited materials were well-crystallized, uniform, smooth and cubic CdS thin films. Furthermore, the grain sizes obviously increased and the optical property was greatly improved with increasing the annealing temperature.