Abstract:0.70Pb(Ni1/3Nb2/3)O3-0.30PbTiO 3-xNiO (x=0, 0.01, 0.015, 0.02, 0.03) ferroelectric ceramics were synthesized by the columbite precursor method. Their structure, dielectric and ferroelectric behaviors were investigated. X-ray diffraction results demonstrate that the satuation of exceesive Ni dissolving into PNN-PT ceramics is no more than lmol%. Examination of the dielectric behavior reveals that the moderate excessive content of Ni and annealing can significantly improve the dielectric property of PNN-PT ceramics. In addition, the excessive content of Ni can also decrease the ferroelectric properties and dispersion behavior of PNN-PT ceramics.