Abstract:Sm-doped ceria (SDC) powders were prepared by aging the solutions of corresponding nitrate salts in the presence of urea and calcining. The effects of the concentration of metal ions and urea on the properties of the resulting precipitates were studied. The mass loss of the precipitation on calcinations was evaluated by UFA- TG. The morphology and structure were investigated by TEM and XRD. The experiment results show that the metal bicarbonates are easily converted to relative oxides by calcination at 500-750 t without any change in morphology. Bulk density of the pressed pellet sintered at 1 500 t exceeds 95 % and the conductivity of the sample is 0.07 S'cm-1 measured by ac impedance spectroscopy at 800 C .