Fracture Mechanisms of Sandwiched Dispersion Fuels

王习术,徐勇,邓燕红
DOI: https://doi.org/10.3321/j.issn:1000-0054.2002.08.028
2002-01-01
Abstract:U 3Si 2-Al is a recently developed dispersion fuel used in research reactors with a complicated production process that requires a special production environment. The mechanical properties of U 3Si 2-Al, which depend to a considerable extent upon the production conditions, are of great significance for the reliability and performance of the reactors. The microstructure morphology of the fracture surfaces of fuel plates under tension was investigated using the SEM technique. The structural features of the pellets and the claddings were analyzed to relate the tensile strength and the configuration of the fuel plate fracture surfaces. Fuel failure was found to be associated with brittle fracture of the pellet core, which leads to plastic collapse of the cores was a predominate parameter in the load-bearing capacity of the fuels plates. The elongation ratio of U 3Si 2-Al is less than that of unannealed cast aluminum.
What problem does this paper attempt to address?