Annealing Crystallization and Catalytic Performance of Ultrafine Ni-B and Ni-Ce-B Amorphous Alloys

XG Wang,XY Zhang,ZR Li,WJ Zhong,B He,SQ Wei
DOI: https://doi.org/10.3321/j.issn:0253-9837.2001.04.020
2001-01-01
Abstract:The structural evolution of ultrafine Ni-B and Ni-Ce-B amorphous alloys annealed at different temperatures was studied by XAFS, DTA and XRD techniques. The benzene hydrogenation was used to characterize the catalytic activity of the Ni-B and Ni-Ce-B alloys. The results indicate that the benzene conversion over the Ni-B and Ni-Ce-B samples reaches their maximum of 63% and 81%, respectively, at the annealing temperature of 623 K. Addition of a small amount (0.3%) of Ce can greatly improve the catalytic activity of the Ni-Ce-B alloy. The DTA results show that the crystallization process of the Ni-B amorphous alloy includes two steps (at 598 K and 653 K), while the Ni-Ce-B alloy exhibits four exothermal peaks at 548, 603, 696 and 801 K. The XAFS and XRD results further reveal that the Ni-B amorphous alloy is crystallized to form nanocrystalline Ni and crystalline Ni3B after annealing at 573 K, but only a small amount of crystalline Ni3B is produced in the case of Ni-Ce-B alloy. At the annealing temperature of 673 K, the crystalline Ni3B in the Ni-B starts to decompose into crystalline Ni, and the nanocrystalline Ni aggregates to form crystalline Ni. At 773 K or higher annealing temperatures, the local structure of Ni atoms in the annealed Ni-B alloy is similar to that in Ni foil. The element Ce in the Ni-Ce-B alloy can retard the crystalline Ni3B to be decomposed and make the Ni lattice distorted greatly. We proposed that the catalytic activity of the ultrafine Ni-B and Ni-Ce-B amorphous alloys for the benzene hydrogenation is in the order: nanocrystalline Ni > ultrafine Ni-B amorphous alloy > crystalline Ni greater than or equal to crystalline Ni3B.
What problem does this paper attempt to address?