Enhancement of temperature coefficient of resistivity in La 0.67Ca0.33MnO3 polycrystalline ceramics

Ji Ma,Yunqi Cai,Wenzhang Wang,Qi Cui,Mya Theingi,Hui Zhang,Qingming Chen
DOI: https://doi.org/10.1016/j.ceramint.2013.10.105
IF: 5.532
2014-01-01
Ceramics International
Abstract:La0.67Ca0.33MnO3 polycrystalline ceramics with high temperature coefficient of resistivity (TCR) have been synthesized by the sol-gel method at the sintering temperature of 1450 degrees C and in a sintering time range of 2 h-24 h. The micrographs of the ceramics reveal that the grains grow up from 2 mu m to about 10 mu m with increasing the sintering time. The optimization of the sintering time is found to be a simple and effective way to largely enhance the TCR values of the ceramics. The highest metal insulator transition temperature T-p (272.5 K) and the largest TCR (21.4%) were obtained in the ceramic sintered for 12 h. The reduction of grain boundary and resistivity contributes to the enhancement of T-p and TCR values. (C) 2013 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
What problem does this paper attempt to address?