Abstract:The TZM alloy plates were prepared by powder metallurgy and rolling method. The microstructure of TZM alloy sintered blank and sheet were observed by metallographic microscope and scanning electron microscope. The results show that sintered blank density is 9.94 g/cm3, the Rockwell hardness is 65 HRC, the microstructure of sintered blank is equiaxed grain, grain uniform distribution, the average grain size is 10 μm and has clear outline of the grain boundary. The density of TZM alloy sheet is 10 g/cm3 after rolling, the tensile strength is 914 MPa and the elongation is 4.6%. Analysis and comparison of the microstructure for the annealed sample under 1000, 1100, 1200, 1300, 1400, 1500 and 1600°C show that the TZM alloy sheet is in the recovery stage at 1000°C, 1100°C, and in start recrystallization state at 1200°C, and fully recrystallized at 1600°C.
What problem does this paper attempt to address?