Hot Compression Deformation Of An Mg-2.54nd-0.26zn-0.32zr Alloy

Honghui Liu,Zhiliang Ning,Fuyang Cao,Jianfeng Du,Jianfei Sun
DOI: https://doi.org/10.3139/146.110954
2013-01-01
International Journal of Materials Research
Abstract:The hot compression deformation of an Mg-2.54Nd-0.26Zn-0.32Zr cast alloy was investigated in the 25-400 degrees C temperature range at initial strain fates from 10(-4) s(-1) to 10(-2) s(-1). It was found that strain rate has little effect on true stress when the material was compressed below 250 degrees C. Above this temperature, high strain rates resulted in an increased true stress. The average strain rate sensitivity exponent at higher temperature (300-400 degrees C) was determined to be 0.24 and the calculated activation energy was 185 kJ . mol(-1), which is higher than that of lattice self diffusion of pure Mg. The constitutive equation was established and the Zener-Hollomon parameter was calculated as a function of peak stress. The microstructure of a sample tested at 300 degrees C was analyzed by optical microscopy.
What problem does this paper attempt to address?