Abstract:2,2-bistrifluoromethyl-4,5-difluoro-1,3-dioxole-co-tetrafluoroethylene (PDD-TFE) copolymer is a good candidate to prepare gas separation membranes with excellent permeability due to its free volume characteristics. However, the influence of PDD-TFE copolymer structure on its free volume characteristics is less studied. In this paper, PDD-TFE copolymers with different compositions and molecular weights were synthesized, and their free volume characteristics were analyzed by positron annihilation lifetime spectroscopy and a molecular dynamics simulation. It indicated that the molar fraction of PDD in copolymers had a significant effect on free volume characteristics, while the molecular weight of copolymers exerted a slight influence on free volume when the molecular weight exceeded a critical region (intrinsic viscosity [eta] > 68 ml g(-1)). PDD-TFE copolymers with greater PDD molar fractions (i.e., 72% and 84%) showed bimodal distributions in positron lifetime and free volume size distributions, while PDD-TFE copolymers with lower PDD molar fractions (i.e., 27% and 35%) exhibited a single peak. The long-lifetime parameter tau(3) was assigned to micro-cavities formed by [-(TFE)(y)-PDD-] segments and tau(4) was attributed to micro-cavities formed by [-(PDD)(x)-TFE-] segments. The cis and trans transitions of PDD led to a local multilayer spiral structure with a 2.6-4.3 angstrom layer spacing, which would also increase the free volume of copolymers.