Fabrication and Properties of the Potassium Sodium Niobate/Cobalt Copper Ferritemultiferroic Magnetoelectric Composites

Xuan Min-Jie,Liu Xin-Yu,Yuan Chang-Lai,Xu Ji-Wen,Ma Jia-Feng
DOI: https://doi.org/10.3724/sp.j.1077.2012.12014
2012-01-01
Abstract:(1-x)(0.9462K(0.5)Na(0.5)NbO(3)-0.0498LiSbO(3)-0.004BiFeO(3))-xCo(0.85)Cu(0.15)Fe(2)O(4)((1-x)(KNN-LS-BFO)-xCCFO) (x=0.1, 0.2, 0.3, 0.4, 0.5) multiferroic magnetoelectric ceramics were prepared by solid phase method. The presence of perovskite and spinel in the sintered composites were proved by XRD patterns and no impurity phase existed. SEM images show that particle size of KNN-LS-BFO is big and complete, while the particle size of CCFO is small. When x increases from 0.1 to 0.5, the piezoelectric coefficient of the composites decreases from 120 pC/N to 33 pC/N, While saturation magnetization and remanent magnetization increase and saturation magnetostriction constant increases from 18x10(-6) to 52x10(-6) approximately. When the applied magnetic field increases, the magnetoelectric properties of the composites increase to the maximum and then decrease. When the alternating magnetic field frequency is 1 kHz and x=0.3, the magnetoelectric voltage coefficient attains maximum value 20.6 mV/A.
What problem does this paper attempt to address?