Novel Fabrication of Injection-Moulded Ceramic Parts with Large Section Via Partially Water-Debinding Method

Wei Liu,Xianfeng Yang,Zhipeng Xie,Cui Jia,Linlin Wang
DOI: https://doi.org/10.1016/j.jeurceramsoc.2012.03.005
IF: 5.7
2012-01-01
Journal of the European Ceramic Society
Abstract:In this work, we adopt a combination of low molecular weight PEG (L-PEG) and high molecular weight PEG (H-PEG) as water-soluble binder to fabricate injection-moulded ceramic parts with large section. The mechanism of the combination of PEGs removal was proposed for the first time. Defect-free near gear parts with large-sized-section (thickness – 16mm) were successfully fabricated through water extraction (15h) followed by rapid thermal pyrolysis (4.5h). It solves the difficulty of fabricating injection-moulded ceramic parts with large section and our approach is energy saving and high-efficiency as compared with conventional thermal debinding. The results demonstrate that our approach of partially water-debinding followed by rapid thermal pyrolysis could solve the problems of conventional thermal debinding, providing an effective route for the production of injection moulded ceramic parts with large section.
What problem does this paper attempt to address?