Consolidation and Mechanical Properties of Cu46Zr42Al7Y5 Metallic Glass by Spark Plasma Sintering

Z. H. Chu,H. Kato,G. Q. Xie,G. Y. Yuan,W. J. Ding,A. Inoue
DOI: https://doi.org/10.1016/j.jnoncrysol.2012.02.027
IF: 4.458
2012-01-01
Journal of Non-Crystalline Solids
Abstract:Cu46Zr42Al7Y5 metallic glass with nearly 100% relative density was obtained by spark plasma sintering (SPS) with a diameter of 15mm, which was larger than the largest size of 10mm for the as-cast specimen. The fracture strength of the sintered specimen reached 2044MPa, which was 15% higher than that of the as-cast Cu46Zr42Al7Y5 glassy specimen. The densification and compressive properties of the sintered specimens were related to sintering temperature. Structural changes of the specimens sintered at various sintering temperatures resulted in the difference of macro-mechanical properties.