Abstract:In the present work, the dependence of microstructure and electrical properties on B-site non-stoichiometry (excess) for (Na0.474K0.474Li0.052)(Nb0.948Sb0.052)O-3-xTa(2)O(5) (KNLNSTx) was symmetrically investigated. The phase structure was pure perovskite when x<0.02 mol. While x>0.02 mol, a secondary phase would be found in the samples. The results indicate that the densification and piezoelectricity were promoted as x<0.01 mol. It is supposed that the low amount of Ta could induce A-site vacancy and favor the poling efficiency. KNLNSTx ceramics with x=0.005 mol Ta2O5 have optimum electrical properties: d(33)=253 pC/N, k(p)=0.437, Q(m)=43 and tan delta=0.027. (C) 2012 Elsevier B.V. All rights reserved.