Abstract:Ce0.8Sm0.2O1.9 (SDC) powder is synthesized by a simplified carbonate coprecipitation method, and the powder can be sintered to densify at 1100–1200°C. SDC sintered at 1200°C exhibits 98.6% of the theoretical density and an effective conductivity (σeff) of 0.038Scm−1 at 700°C. Arrhenius plots of log(σeffT) vs. 1/T for SDC sintered between 900 and 1300°C are curved at about 600°C, giving activation energies of ∼0.9eV below 600°C and ∼0.8eV above 600°C. SDC sintered at 1400°C, however, shows decreased σeff with a higher activation energy of ∼1.0eV independent of temperature within 400–800°C, and pinholes appear at tri-junctions of grain boundaries because of reduction of CeO2 at high temperatures.