Effects of Cold Working Degrees on Grain Boundary Characters and Strain Concentration at Grain Boundaries in Alloy 600

J. Hou,Q. J. Peng,Z. P. Lu,T. Shoji,J. Q. Wang,E. -H. Han,W. Ke
DOI: https://doi.org/10.1016/j.corsci.2010.11.022
IF: 7.72
2011-01-01
Corrosion Science
Abstract:Strain concentration at grain boundaries and grain boundary microstructure in cold worked Alloy 600 were characterized. Excluding the annealing twin boundaries, the base and 20% cold worked alloys exhibited higher random grain boundary fractions than the 8% and 40% cold worked alloys. An increased low angle boundaries and decreased annealing twins were observed with deformation. The 20% cold worked alloy displayed a maximum strain concentration at grain boundaries. The stress corrosion cracking growth in cold worked Alloy 600 in high temperature water showed a strong correlation with the strain concentration at grain boundaries.