Effects of the proportion of nano-diamond and zirconia on the color of core resin

LUO Juan,LIU Xueheng,WANG Xinzhi
DOI: https://doi.org/10.3969/j.issn.1003-7632.2008.03.008
2008-01-01
Abstract:Objective Add zirconia and nano-diamond into the photocurable composite resin matrix which main filler is barium glass,then the influence of the color is observed.Methods Bis-GMA and TEGDMA are resin matrix,BG is filler.Different content of nano-zirconia or micro-zirconia and UFD,mixed with main filler barium glass,are added into resin matrix to fabricate photocurable composite core materials,six groupe resins of which flexural strength can reach the corresponding national and ISO criteria are chosen,then the color differences(△E)between resins and 63 natural dentin are taken with Shade Eye Colorimeter(Shofu).Results The CIELab values of resins are beside 63 national tooth dentin color dimension.△E between two of thus are 5.6~12.24.Conclusion The color differences between resins by ourselves and 63 tooth dentin can be taken in clinic.The resins can meet the requirement of esthetic to repair initial tooth defect.
What problem does this paper attempt to address?