Preparation of HPEEK by Oligomer A2+B3 Approach

Jianxin Mu,Guibin Wang,Chunling Zhang,Xiujie Li,Zhenhua Jiang,V. V. Kireev
DOI: https://doi.org/10.1080/10601320802222681
2008-01-01
Abstract:A series of hyperbranched poly(ether ether ketones) with different chain length between branching point (L) were prepared using a A(2)+B-3 methodology, in which the A(2) is hydroxyl-terminated PEEK oligomer. The L affects the properties of the polymers such as the inherent viscosity, the degree of crystallinity, the thermal properties of the polymers etc. The polymer with a L-2 approximate to 8 had T-g (122.4 degrees C), T-c (200.2 degrees C), and broad T-m (247.4 degrees C). With the increment of L, up to the point L-2 approximate to 20 and L-2 approximate to 35, the polymers become semi-crystalline, with a melting point of 300.9 degrees C and 317.9 degrees C, respectively. Their wide angle X-ray scattering (WAXS) pattern indicated that their crystal structure is exactly the same as that of the linear homopolymer.