Effect of Bi2O3 Adding and Sintering Temperature on the Cut-off Frequency of NiZn Ferrites

孔占兴,梁迪飞,谢建良,邓龙江
DOI: https://doi.org/10.3969/j.issn.1001-3830.2008.06.015
2008-01-01
Abstract:Ni0.25Co0.14Cu0.4Zn0.21Fe1.98O4 ferrite was prepared using different amount of Bi2O3 as latent solvent by common ceramic process.X-ray diffraction(XRD) and scanning electron microscopy(SEM) were used to analysize the phase composition and observe the microstructure of samples,respectively.The permeability spectrum was measured by impedance analyzer to inspect the effect of Bi2O3 latent solvent and sintering temperature on the cut-off frequency of the samples.A cut-off frequency of 1GHz was achieved for initial permeability of 5.5.Sintering temperature can be decreased to 850℃ when adding 4wt% Bi2O3 latent solvent.