Influences of Bi2O3 Additive on the Microstructure, Permeability, and Power Loss Characteristics of Ni–Zn Ferrites

Hua Su,Xiaoli Tang,Huaiwu Zhang,Lijun Jia,Zhiyong Zhong
DOI: https://doi.org/10.1016/j.jmmm.2009.05.046
IF: 3.097
2009-01-01
Journal of Magnetism and Magnetic Materials
Abstract:Nickel–zinc ferrite materials containing different Bi2O3 concentrations have been prepared by the conventional ceramic technique. Micrographs have clearly revealed that the Bi2O3 additive promoted grain growth. When the Bi2O3 content reached 0.15wt%, a dual microstructure with both small grains (<5μm) and some extremely large grains (>50μm) appeared. With higher Bi2O3 content, the samples exhibited a very large average grain size of more than 30μm. The initial permeability gradually decreased with increasing Bi2O3 content. When the Bi2O3 content exceeded 0.15wt%, the permeability gradually decreased with frequency due to the low-frequency resonance induced by the large grain size. Neither the sintering density nor the saturation magnetization was obviously influenced by the Bi2O3 content or microstructure of the samples. However, power loss (Pcv) characteristics were evidently influenced. At low flux density, the sample with 0.10wt% Bi2O3, which was characterized by an average grain size of 3–4μm and few closed pores, displayed the lowest Pcv, irrespective of frequency. When the flux density was equal to or greater than the critical value of 40mT, the sample with 0.20wt% Bi2O3, which had the largest average grain size, displayed the lowest Pcv.
What problem does this paper attempt to address?