Preparation and MRI Characteristics of Supraparamagnetic Ironic Oxide-Loaded Polymeric Nano-Vesicles
FENG Shi-ting,LI Hao,SUN Can-hui,PAN Bi-tao,QIU Peng-xin,SHUAI Xin-tao,LI Zi-ping,MENG Quan-fei
DOI: https://doi.org/10.3760/cma.j.issn.1674-1927.2011.06.006
2011-01-01
Abstract:Objective To prepare the polymeric nano- vesicles loaded with hydrophobic and hydrophilic supraparamagnetic ironic oxide (SPIO) and to investigate their physical,chemical and MRI characteristics.Methods The polymeric nano-vesicles were prepared from poly D,L-lactic acid (PDLLA)and poly ethylene glycol (PEG) by a multiple emulsion/solvent evaporation method.The hydrophobic SPIO and hydrophilic SPIO were loaded in the polymeric nano-vesicles respectively.Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were used to demonstrate the size,distribution and morphous of the SPIO-loaded polymeric nano-vesicles.The MRI T2 relaxivities (1/T2) of water-soluble SPIO,hydrophobic SPIO-loaded and hydrophilic SPIO-loaded vesicles at different concentrations (stock solution,1/2,1/4,1/8,1/16,1/32 of stock solution respectively) were measured by T2 map sequence and T2 mapping software.Results The average diameter of the hydrophobic SPIO loaded polymeric nano- vesicles was (182.2±23.9) nm,compared with (191.7±28.7) nm for the hydrophilic SPIO loaded nano-vesicles.SME and TEM showed that the hydrophobic SPIO particles were uniformly dispersed in the membrane of the vesicle,while clusters of the hydrophilic SPIO particles were loaded in the inner core of the vesicles.The T2 relaxivity rates (1/T2) of water-soluble SPIO at different concentrations were 7.18,4.96,3.02,2.11,1.92 and 1.81,respectively.The T2 relaxivity rates of hydrophobic SPIO-loaded vesicles at different concentrations were 14.45,9.60,4.15,2.85,2.40 and 2.10,respectively.The T2 relaxivity rate of hydrophilic SPIO-loaded vesicles at different concentrations were 9.44,13.02,6.95,4.60,3.13 and 2.53,respectively.Conclusions The SPIO-loaded vesicles are more superparamagnetic than those of water-soluble SPIO at the same concentration of SPIO.The hydrophilic SPIO-loaded polymeric nano-vesicles have a higher MRI T2 relaxivity rate than hydrophobic SPIO-loaded vesicles.