Measuring the Fatigue Life of Porcelain Fused Metal Crown and Bridge of Posterior Teeth

LI Ming-yong,MA Xuan-xiang,LI Yu-long,LI Zhun,AI Lin,ZHOU Zhang-hua,ZHANG Hai-xia
DOI: https://doi.org/10.3969/j.issn.1008-6455.2011.06.044
2011-01-01
Abstract:Objective To measure the fatigue life of porcelain fused metal(PFM) crown and bridge of posterior teeth.Methods PFM crown and bridge of anterior teeth were made for measurement of its fatigue life.The surface of porcelain on bitting area were observed by stereoscopic zoom microscopes after 0h、16h、48h、80h、160h,and by scaning electric microscopes(SEM) after 320h.Results Each PFM crown and bridge of posterior teeth had no procelain cracks in evidence after experiment,however there were some microscopic wears among 30~50μm appeared on the surface of functional area by SEM after simulating mastication 20 years.Conclusion PFM restorations of posterior teeth have rather fine mechanics characteristic.It may last 20 years even longer by using normal masticatory force.
What problem does this paper attempt to address?