Abstract:We report on the atomic layer deposition (ALD) of MnO and NiO thin films on Si(100) using Mn(EtCp)2 [EtCp=ethylcyclopentadienyl, (C2H5)C5H4] and Ni(EtCp)2 in the temperature range of 150–300°C. H2O or O3 is selected as oxygen source for the depositions. The growth temperature (Tg) and oxygen source impact on the structure, electronic density, and impurity concentration for the as-grown MnO and NiO films have been studied using X-ray reflectivity (XRR), grazing incidence X-ray diffraction (GIXRD), and Fourier transform infrared (FTIR) spectroscopy. A steady growth rate of 0.024–0.025nm/cycle for the films grown using Mn(EtCp)2 and H2O was observed in the Tg range of 250–300°C. FTIR does not show any carbon impurities in the MnO films grown with H2O. The films grown using Mn(EtCp)2 and O3 at 300°C exhibit poor adhesion on Si(100). NiO films with low amounts of contaminants are achieved using O3 and at a Tg of 250°C or above. The growth rate, however, is very high for films deposited at Tg=150°C and decreases significantly in films deposited at higher temperatures. In addition, no film growth was observed for the Ni(EtCp)2/H2O process. The as-grown MnO and NiO films prepared using H2O and O3 as oxidizer, is shown, by GIXRD a polycrystalline cubic structure.
What problem does this paper attempt to address?