Design of Phase-containing Particles with Core-shell Morphology and Their Toughening Condition on POM Resin

于建,张良方,郭朝霞
DOI: https://doi.org/10.3321/j.issn:1001-9278.2002.02.005
2002-01-01
Abstract:For POM/TPU/CaCO3 composite system, the phase-containing particles with CaCO3 as the core and TPU as the shell were achieved automatically by means of inducing TPU to coat CaCO3, and the particles could increase the toughness of POM resin effectively. The processing procedure is very simple and the mechanical properties of the composite material are comparable with POM/TPU alloy. More importantly, it was firstly demonstrated that using rigid inorganic particles with elastic shell to toughen polymer matrix, the brittle-ductile transition rule depended not only on interparticle distance, but also on shell thickness of the toughening particles. For POM resin, the composite system could not arrive B-D transition until at a critical interparticle distance Tc(Tc≤0.18 μm) and at a critical shell thickness Lc(Lc≥0.7 μm). Once meeting the critical condition, the notch impact strength of the material was ten times greater than that of POM resin, and the tensile strength could reach around 30 MPa.
What problem does this paper attempt to address?