Low-Temperature Synthesis of Hollow ?-Tricalcium Phosphate Particles for Bone Tissue Engineering Applications
Iman Roohani,Young Jung No,Betty Zuo,Sue D Xiang,Zufu Lu,Hongwei Liu,Magdalena Plebanski,Hala Zreiqat
DOI: https://doi.org/10.1021/acsbiomaterials.1c01018
2022-01-01
ACS Biomaterials Science & Engineering
Abstract:beta-Tricalcium phosphate (beta-TCP) has been exten-sively used in bone tissue engineering in the form of scaffolds,granules, or as reinforcing phase in organic matrices. Solid-statereaction route at high temperatures (>1000 degrees C) is the most widelyused method for the preparation of beta-TCP. The high-temperaturesynthesis, however, results in the formation of hard agglomeratesand fused particles which necessitates postprocessing steps such asmilling and sieving operations. This, inadvertently, could lead tointroducing unwanted trace elements, promoting particle shapeirregularity as well as compromising the biodegradability andbioactivity of beta-TCP because of the solid microstructure ofparticles. In this study, we introduce a one-pot wet-chemicalmethod at low temperatures (between 160 and 170 degrees C) to synthesize hollow beta-TCP (h beta-TCP) submicron particles of an averagesize of 300 nm with a uniform rhombohedral shape. We assessed the cytocompatibility of the h beta-TCP using primary humanosteoblasts (HOB), adipose-derived stem cells (ADSC), and antigen-presenting cells (APCs). We demonstrate the bioactivity of theh beta-TCP when cultured with HOB, ADSC, and APCs at a range of particle concentrations (up to 1000 mu g/mL) for up to 7 days. h beta-TCP significantly enhances osteogenic differentiation of ADSC without the addition of osteogenic supplements. These findings offera new type of beta-TCP particles prepared at low temperatures, which present various opportunities for developing beta-TCP based biomaterials