Influence of Working Conditions and Blank Sizes on Low Temperature Impact Properties of 35CrMo Steel

ZHU Yue-feng,YIN Yong-jing,ZHAO Xu-ping,HE Zhuo-zuo,ZHANG Yong,LIU Jian
DOI: https://doi.org/10.3969/j.issn.0254-6051.2006.03.022
2006-01-01
Abstract:According to the service conditions of petroleum devices at low temperature,the impact properties of 35CrMoA steel and cast steel ZG35CrMo applied commonly in petroleum industry and the effects of the processing conditions,blank sizes,and temperature were respectively studied.The results of the impact tests showed that the impact properties of 35CrMoA steel and cast steel ZG35CrMo decreased with the decreasing test temperature and there existed a ductile-brittle transition between -30℃ and 0℃.The effect of the blank sizes on the impact properties of 35CrMoA steel was evident under the conventional heat treatment conditions.The specimens cut from the blanks with moderate sizes (130mm) displayed good impact properties,particularly at ambient and moderately low temperatures from -20℃ to 20℃,and the impact properties of the specimens from both small (60mm) and big (220mm) blanks were remarkably decreased.It was demonstrated that moderate cooling rates during the heat treatments would be beneficial to improve the impact properties of steels.The impact properties of the cast steel ZG35CrMo at low temperatures,especially between -60℃ and -40℃,were almost same as that of 35CrMoA steel,which indicated that impact properties of 35CrMo steels were sensitive to the processing conditions only at ambient and moderate low temperatures.It should be mentioned that,with the test temperature decreased from -20℃ to -60℃,the impact property decrease amplitude of the cast steel ZG35CrMo was much smaller than that of 35CrMoA steel.In addition,the impact fractures of both 35CrMoA steel and cast steel ZG35CrMo revealed similar characteristics at every corresponding test temperatures.
What problem does this paper attempt to address?