Magnesium Leaching Behavior from a Copper Tailing with Hydrochloric Acid

Feng Yali,Yang Zhichao,Li Haoran,Teng Qing,Wang Weida,Zhou Yuzhao
2013-01-01
Abstract:In order to efficiently develop and utilization of magnesium from high-magnesium copper tailings,technical conditions for the hydrochloric acid leaching process were studied,and the leaching kinetics model was established. The results showed that under conditions of hydrochloric acid 1 mol / L,reaction temperature at 353 K,liquid to solid ratio of 3∶ 1,reaction time 4 h,stirring speed of 300 r / min,the magnesium leaching rate reached 75. 55%; Avrami model can better describe the leaching process. XRD,SEM analysis of leaching residue under different conditions showed that: when the magnesium leaching rate is 75%,the serpentine's structure has been completely destroyed,thus diffraction peaks of serpentine in leaching residue disappeared; High temperature and high pressure only makes the crystal structure of some calcium-magnesium garnets unstable and reaction with hydrochloric acid,which is the reason for lowering the leaching rate of magnesium acid.
What problem does this paper attempt to address?