Study on Extracting Vanadium from Stone Coal Calcine by Pressure Alkaline Leaching

Xiao Chao,Xiao Liansheng,Ding Wentao
2010-01-01
Abstract:Considering that extracting V2O5 from coal-stone by "roasting-alkali leaching " process exist some serious problems such as abundant alkali consumption,long leaching time and leaching solution with high impurity content and so on,the experiment of extracting V2O5 from stone coal calcine by pressure alkaline leaching was investigated,and effects of dosage of sodium hydroxide,liquid-solid ratio,leaching time,recycle leaching on the vanadium leaching were studied.The results showed that when sodium hydroxide 3.5% of ore calcine weight,the ratio of liquid-solid 1.5∶1,leaching temperature 180 ℃,leaching time 2 h,the leaching rate of vanadium in stone coal is 86%,mass ratio of vanadium and silicon is 0.65,and pH of the leaching solution is 12.1.High-pressure alkaline leaching process with the advantage of high leaching rate of vanadium but low leaching rate of other impurities,provides a new way for extracting V2O5 from stone coal.
What problem does this paper attempt to address?