Research on Properties of Co-Free AB_5-Type Hydrogen Storage Alloys by Addition of a Little Si

Dong Hui,Wei Xuedong,Liu Yongning,Zhu Jiewu,Lin Jianxiong,Wen Ying
DOI: https://doi.org/10.3321/j.issn:1002-185X.2008.01.037
2008-01-01
Rare Metal Materials and Engineering
Abstract:La(NiAlMn)(5-x)Si-x (0 <= x <= 0.35) alloys were prepared by inductive melting. The crystal structure of alloys was determined by X-ray and SEM, and the electrochemical properties were also investigated The results show that the alloys are composed of LaNi5 as main phase, while x < 0.3.When x=0.35, the alloy is composed of LaNi5 as matrix and LaNi3 as secondary phase. With the increase of Si content the maximum discharge capacity and the high rate discharge (HRD) ability decrease gradually, however the cycle stability is improved correspondingly. The lowest capacity decay can remain 19.4 % (x=0.35) after 3,00 charge/discharge cycles. The lower corrosion current densities of the Si-containing alloys can be explanation for the good cycle life of them.
What problem does this paper attempt to address?