Abstract:Objective To evaluate the bond strength of resin coating material of Hybrid Coat(HyC) to dentin.Methods A group(HyC) and other three kinds of dentin adhesives,B group(G-Bond)、C group(Mega Bond) and D group(Single Bond) were selected and applied to bovine teeth according to manufacturers' instructions.The shear bond strength of each specimen was measured and analyzed with Tukey-Kramer Test(p0.05).Stereomicroscope was used to observe the fracture modes.Results B,C and D groups showed higher bond strength,but there was not any significant difference among them.A group(HyC) showed the lowest strength of about 10.08 MPa,and there was significant difference between A and the other three groups.Stereomicroscope examination indicated that the adhesive failure was the most mode of fracture in A group and cohesive failure and mixed failure were the main mode of fracture in B,C and D groups.Conclusion The three kinds of dentin bond agents showed higher shear bond strength than HyC.It is necessary to enhance the bond strength of HyC to dentin in the following research to ensure the long-term effectiveness of dentin coating technique.
What problem does this paper attempt to address?