Abstract:Friction stir spot welding with Com-stirTM was adopted to make lap joints on the thin aluminum alloy board LF21 with a thickness of 2 mm.The shearing resistance was tested at different rotary radius.Furthermore,the fracture path and the microstructure were observed and analyzed.Experimental results show that the fracture path of FSSW joint can vary with the rotary radius.Keeping other parameters constant,the maximum shearing resistance 3.47 kN of the joint can be realized when the rotary radius reaches 1 mm.At the same time,the joint surface is bright and beautiful at this rotary radius.The metallographic structure shows that the metal flows intensively in the stirred zone and the TMAZ area,in which the grain size is fine and the structure is compact.