Densification kinetics and sintering behaviour of a Ti(C0.7N0.3)-WC-Mo2C–NbC-(Co,Ni) compact
Hao-Jun Zhou,Ming-Chu Huang,Hao Yang,Hong-Liang Tao,Yu-Hang Yin,Feng-Hua Luo
DOI: https://doi.org/10.1016/j.jallcom.2020.156072
IF: 6.2
2020-11-01
Journal of Alloys and Compounds
Abstract:In order to understand the densification kinetics of a Ti(C0.7N0.3)-WC-Mo2C–NbC-(Co, Ni) compact, the linear shrinkages were measured using a horizontal dilatometer at different heating rates (2, 4, and 6 °C/min) in an argon atmosphere. Densification is more efficient when it is sintered at a lower heating rate. A master sintering curve was constructed over a range from the relative density of approximately 0.658–0.816; the corresponding sintering activation energy was 630 kJ/mol. With the aid of an Arrhenius curve, the sintering behaviour of cermet was analysed at different temperatures. The sintering process changed from solid-phase to liquid-phase sintering at approximately 1385 °C. The sintering activation energy turned negative when the temperature exceeded 1385 °C at a heating rate of 2 °C/min due to the formation of a liquid phase, and the exothermic process of dissolution-precipitation.
materials science, multidisciplinary,chemistry, physical,metallurgy & metallurgical engineering