Preparation, Characterization and Photocatalytic Activity of Flowerlike Cadmium Sulfide Nanostructure

Xu Di,Sushil K. Kansal,Wenli Deng
DOI: https://doi.org/10.1016/j.seppur.2009.04.007
IF: 8.6
2009-01-01
Separation and Purification Technology
Abstract:Flowerlike cadmium sulfide (CdS) nanostructure was prepared via the controllable solvent thermal method by using ethylenediamine as the structure directing template. The synthesized CdS was characterized by X-ray diffraction (XRD) and scanning electron microscopy (SEM). XRD pattern showed that the flowerlike CdS nanostructure was a cubic cell. SEM images showed that flowerlike CdS nanostructure is built from dozens of petals. The average crystal size was calculated to be about 3.1nm. The petals were about 30nm thick and 1μm wide. The specific surface area of flowerlike CdS nanostructure was found to be 20.77m2g−1, higher than CdS powder (10.18m2g−1). Photoluminescence (PL) spectrum revealed that CdS nanostructure had a visible blue emission peak at the wavelength of 433nm, which arises from the excitonic emission. The photocatalytic activity of CdS was investigated for the decolorization of methyl orange (MeO) under high-pressure mercury lamp illumination. It was observed that the flowerlike CdS showed better results as compared to other CdS materials.
What problem does this paper attempt to address?