Effect of 125I Seeds Irradiation on Biodegradation Properties and Biocompatibility of Chitosan-Coated PGLA Carrier in Vivo

YU Lei,CHEN Hong-hong,TAN Zhi-qing,JIANG Xun,HU Yu-xing,WANG Wen-zhu,CHENG Wen-ying
DOI: https://doi.org/10.3969/j.issn.1672-8467.2007.02.015
2007-01-01
Abstract:Purpose To evaluate the effect of continuous low-dose-rate irradiation delivered by 125I seeds on degradation behavior and biocompatibility of chitosan-coated poly (lactic-glycolic acid) (PGLA) brachytherapy seeding carrier in vivo. Methods The chitosan-coated PGLA carrier loaded with two 125I seeds was implanted into latero-spinal muscle of Sprague Dawley rat. The apparent radioactivity of each 125I seed was 29.6 MBq. The weight loss and morphology change of the coated PGLA carrier were monitored at different degradation time. The tissue of the implanted site was observed by light microscopy (LM) and transmission electron microscopy (TEM). X-ray photography was performed regularly to evaluate seeds migration. Results Two weeks after implantation, the weight loss of PGLA carrier irradiated by 125I seeds was about 13%, which was not significantly different from that of the control group. Three weeks after implantation, the weight loss of irradiated group reached 41% and broken filaments and blur structure were observed, showing faster degradation rate than the control group. But the structure integrity and a certain degree of strength of the coated PGLA carrier remained. There were large mounts of fibrous tissue accrementition around the carrier sheet. Four weeks after implantation, 125I seed carrier sheet was completely encapsulated and fixed by peripheral dense connective tissue and was difficult to detach from each other. LM and TEM observation on tissue of implanted site indicated that there were many inflammatory cells within 2 weeks post implantation and a little inflammatory cells 4 weeks after implantation. The pores in the degradated PGLA carrier were filled with fibroblasts and collagen fibers. The amount of macrophages increased and phagocytosis were obvious. Neogenesis of the skeletal muscle cells was observed and no abscessus and necrosis was found. There were no significant difference between the radiation group and control group. X-ray photography exhibited that the spatial location between the two 125I seeds and between the 125I seeds and bony structure of the rat didn't change significantly 2h, 3 day, 1 week, 2 weeks, 3 weeks and 4 weeks after implantation. Conclusions The chitosan-coated PGLA carrier can maintain the spatial distribution of 125I seeds and their biocompatibility in rats. It is safe and effective to be used in brachytherapy.
What problem does this paper attempt to address?