Preparation of Ag-embedded Nano-Tio_2 Antibacterial Agent

MA Deng-feng,PENG Bing,CHAI Li-yuan,WEI Shun-wen,WANG Ja,CAI Lian-bing
DOI: https://doi.org/10.3969/j.issn.1009-9212.2006.01.022
2006-01-01
Abstract:In this study,precursor of nano-TiO2 was prepared from industrial H2TiO3 and 98% sulfuric acid in continuous acid dissolution and pyro-hydrolysis.The precursor was embedded with silver in the form of Ag3PO4.The optimum parameters for the preparation was the ratio of H2TiO3 to H2SO4 in dissolving process=3 and time=150-180 min,hydrolysis time=100-120 min.After dried with a sprayer and thermal treated at 450 ℃,500 ℃ and 550 ℃,the TiO2 present in the product was in anatase phase and without simple silver saline phase based on the analyses of X-ray Diffraction(XRD).The particle size of product Ag-embedded nano-TiO2 was in the range of 20~80 nm.The minimum inhibitor concentration(MIC) of the product was 100 ppm and the efficiency of sterilization was 99.99%.
What problem does this paper attempt to address?