Effect of MnO 2 Addition on the Electrical Properties of PNZST Ceramics
Yangxi Yan,Hongliang He,Yujun Feng
DOI: https://doi.org/10.1007/s11664-014-3106-5
IF: 2.1
2014-01-01
Journal of Electronic Materials
Abstract:(Pb 0.99 Nb 0.02 )[(Zr 0.70 Sn 0.30 ) x Ti 1− x ] 0.98 O 3 (PNZST) piezoelectric ceramics of pure perovskite structure were prepared by a conventional ceramic fabrication method, where x = 0.48–0.56. When x = 0.52, the ceramics exhibit a high piezoelectric coefficient ( d 33 ∼ 490), but the mechanical quality factor ( Q m ) is only 72. To increase the Q m and not dramatically lower the d 33 , MnO 2 was chosen as the additive. The effects of adding MnO 2 on the sinterability, structure, and electrical properties of PNZST ceramics were investigated in detail. With a small addition of MnO 2 (≤0.6 wt.%), the Mn ions are homogeneously dissolved in the PNZST ceramic, leading to full densification when sintered at 1,300 °C. However, further addition of MnO 2 prevents densification, causing a high porosity and small grain size. The doping of MnO 2 transforms the phase structure from tetragonal to rhombohedral. The addition of MnO 2 up to a maximum of 0.6 wt.% remarkably improves the mechanical quality factor ( Q m ) of PNZST ceramics, simultaneously as well as maintaining a high d 33 and k p . PNZST with 0.6 wt.% MnO 2 exhibits excellent electrical properties with piezoelectric coefficient d 33 = 392 pC/N, electromechanical coupling factor k p = 0.60, mechanical quality factor Q m = 1,050, dielectric constant ε r = 1,232, dielectric dissipation tan δ = 0.0058, and Curie temperature T C = 300 °C.