Synthesis and Characterization of Poly[(methylsilyleneethynylenephenyleneethynylene)s-co-decamethylpentasiloxane]

Fei Gao,Lingling Zhang,Yan Zhou,Farong Huang,Lei Du
DOI: https://doi.org/10.1080/10601325.2010.492274
2010-01-01
Abstract:Poly[(methylsilyleneethynylenephenyleneethynylene)s-co-decamethylpentasiloxane] was synthesized by polycondensation reaction of di-Grignard reagent of diethynylbenzene with 1,9-dichlorodecamethylpentasiloxane and dichloromethylsilane. The copolymer is a liquid and soluble in common organic solvent at room temperature. The copolymer was characterized by FTIR, 1H-NMR, rheological analysis, and differential scanning calorimetry. The results show that the copolymer exhibits good processability and cures at about 170 degrees C. The copolymer can be thermally cured to produce highly crosslinked copolymer. The thermal stability of the cured copolymer was measured by thermogravimetric analysis. The degradation temperature at 5% weight loss is 591 degrees C and the residue yield at 1000 degrees C is 86% in N2. Black, hard, and glassy ceramic was produced when the cured copolymer was heated above 1450 degrees C under argon. The ceramic has high thermooxidative stability.
What problem does this paper attempt to address?