Hot deformation behavior and microstructure evaluation of hydrogenated Ti-6Al-4V matrix composite

Junqiang Lu,Jining Qin,Weijie Lu,Yifei Chen,Di Zhang,Hongliang Hou
DOI: https://doi.org/10.1016/j.ijhydene.2009.09.029
IF: 7.2
2009-01-01
International Journal of Hydrogen Energy
Abstract:Ti-6Al-4V matrix composite reinforced with TiB and TiC particulates was prepared and hydrogenated. Isothermal compression tests were carried out at the deformation temperatures ranging from 750°C to 900°C and strain rate ranging from 0.01s−1 to 1s−1. The effects of hydrogen concentration, deformation temperature and strain rate on flow stress-strain curves and microstructure evaluation were studied. Hydrogen decreases the deformation temperature at least 100°C or enables the composite to deform at a higher strain rate at the same flow stress level. Hydrogen improves dynamic recrystallization of α phase and accommodation deformation between reinforcements and matrix. Optimum hydrogen concentrations at different deformation temperatures were determined. The strain rate sensitivity index and apparent activation energy of the composite with 0wt.% H and 0.35wt.% H were calculated and discussed.
What problem does this paper attempt to address?