Abstract:The pyrolytic characteristics of bagasse and poplar timber(Populus spp.)at different heating rates(5~50 ℃/min) under N2 atmosphere(20mL/min) were studied by using thermogravimetric analysis(TG).The result showed that the pyrolysis speed of the studied biomasses increased with the increment of the heating rate.The pyrolysis process of bagasse and poplar timber consisted of four stages,i.e.,drying from dehydration,pre-pyrolysis,fast pyrolysis and slow pyrolysis of the residues.The weight loss of bagasse and poplar timber at the fast pyrolysis stage was about 80 w % and 85 w %,respectively.The pyrolysis process could be described by first-order global model for both biomass materials.With the method of Coasts-Redfern,the average activation energy of bagasse and poplar timber at low temperature pyrolysis stage was 40.84 kJ/mol and 74.94 kJ/mol,whereas 9.21 kJ/mol and 11.39 kJ/mol individually at high temperature stage.The differences in pyrolysis process between bagasse and poplar timber were due to their different chemical components.
What problem does this paper attempt to address?