Effects of Heat Treatments on the Microstructures and Mechanical Properties of Mg–3Nd–0.2Zn–0.4Zr (wt.%) Alloy

Fu Penghuai,Peng Liming,Jiang Haiyan,Chang Jianwei,Zhai Chunquan
DOI: https://doi.org/10.1016/j.msea.2007.08.064
2008-01-01
Abstract:Microstructure and mechanical properties of as-cast and different heat treated Mg–3Nd–0.2Zn–0.4Zr (wt.%) (NZ30K) alloys were investigated. The as-cast alloy was comprised of α magnesium matrix and Mg12Nd eutectic compounds. After solution treatment at 540°C for 6h, the eutectic compounds dissolved into the matrix and small Zr-containing particles precipitated at grain interiors. Further aging at low temperatures led to plate-shaped metastable precipitates, which strengthened the alloy. Peak-aged at 200°C for 10–16h, fine β″ particles with DO19 structure was the dominant strengthening phase. The alloy had ultimate tensile strength (UTS) and elongation of 300–305MPa and 11%, respectively. Aged at 250°C for 10h, coarse β′ particles with fcc structure was the dominant strengthening phase. The alloy showed UTS and elongation of 265MPa and 20%, respectively. Yield strengths (YS) of these two aged conditions were in the same level, about 140MPa. Precipitation strengthening was the largest contributor (about 60%) to the strength in these two aged conditions. The hardness of aged NZ30K alloy seemed to correspond to UTS not YS.
What problem does this paper attempt to address?