In situ reaction synthesis of Ti–TiB composites containing high volume fraction of TiB by spark plasma sintering process

Zhao-hui Zhang,Xiang-Bo Shen,Sai Wen,Jie Luo,Shu-kui Lee,Fu-chi Wang
DOI: https://doi.org/10.1016/j.jallcom.2010.04.218
IF: 6.2
2010-01-01
Journal of Alloys and Compounds
Abstract:The in situ toughened Ti–TiB ceramic–matrix composites containing high volume fraction of TiB were synthesized by spark plasma sintering technique under a pressure of 50MPa, with sintering temperature ranging from 1100°C to 1400°C and heating rate of 150°C/min, using Ti and TiB2 powders. Results indicated that Ti–TiB composites sintered at 1400°C provided the optimal combination of dense microstructure, well developed lath-shaped TiB grains, and excellent mechanical properties, including the relative density of 99.6%, bending strength of 608MPa, and a rather high fracture toughness of 9.35MPam1/2. Moreover, the micro-hardness of the composites reaches a relatively high level (18.3GPa).
What problem does this paper attempt to address?