Effects of microarc oxidation time on bonding strength of titanium to porcelain

LI Jian-Xue,ZHANG Yu-Mei,HAN Yong,LIU Xiao-Chen,YU Fan
2006-01-01
Abstract:AIM:To study the effects of time length of microarc oxidation (MAO) on the titanium-ceramic bonding strength. METHODS: Titanium samples were treated with MAO in a Na_2SiO_3 electrolytic solution with duty cycle 0.04, frequency 500 Hz, and voltage 300 V. According to the different oxidation time, experimental groups consisted of 3, 6, 10 min groups. The non-MAO samples were used as a control group. The surface of the samples was observed by scanning electron microscope (SEM). The samples were bonded to porcelain. The bonding strength of the samples was measured by a three-point bending test. RESULTS: The bonding strength (MPa) of the samples to porcelain in 3, 6, 10 min groups and control group was 56.4± 0.8, 40.4±2.3,36.0±3.0,32.2±1.9. The longer the oxidation time was, the rougher the surface was, the larger the pore diameter was and the fewer the pore was. The thickness of oxidized layer was increased from 5 μm to 12 μm, but the bonding strength of titanium-porcelain was decreased, respectively (3-min group vs 6-min and 10-min group, P<0.01; 6-min group vs 10-min group, P>0.05). The bonding strength of the MAO groups were higher than that of the non-MAO group (P<0.01). CONCLUSION: The MAO on titanium is favorable to the titanium ceramic bonding strength and the different oxidation time has a different effect on the titanium-ceramic bonding strength.
What problem does this paper attempt to address?